Abstract:
In one embodiment, the present invention provides an uncured composite composition. The uncured composite composition includes an uncured resin and a triaxial braid. The triaxial braid includes a longitudinal axis, a first bias fiber extending in a first bias direction at a first bias angle to the longitudinal axis, a second bias fiber extending in a second bias direction at a second bias angle to the longitudinal axis, and an axial fiber extending in a direction parallel to the longitudinal axis; wherein the first bias fiber, the second bias fiber, and the axial fiber have a substantially same tow size, and the tow size is in a range of from about 1 k to about 11 k. A cured composite and a method of making the cured composite are also provided.